Reducing Coarse Particles to Improve Quality
Customer's Problem
The particle size distribution looked good, but after commercialization, quality deteriorated due to residual coarse particles. The customer wants to improve quality.
AIMEX's Proposed Solution
Solution Through Changing Operating Conditions
When coarse particles remain, insufficient impact energy is suspected.The basic approach is to increase the peripheral speed and the bead size.
At the same time, collision frequency must also be sufficient. Without enough frequency to capture coarse particles, they will remain indefinitely.
Solution Through Bead Mill Selection
We recommend the AIMEX Neo-Alphamill. It was developed specifically to drastically reduce residual coarse particles. Its unique high-density bead layer captures coarse particles without letting them escape and grinds them finely.

The first is the high-efficiency dispersion zone created by the Delta-V disc. The disc has no protrusions, so performance does not degrade with wear, and it moves small beads efficiently for high grinding and dispersion performance.
The second is the high-density bead layer. It forms where the high-efficiency dispersion zone meets the downward force on the beads from the centrifugal separator blades above it. Because the beads move slowly and densely in this layer, coarse particles are reliably captured without escaping.

Coated surface: conventional mill

Coated surface: Neo-Alphamill

Although particle size distributions were nearly the same, the coated surface evaluation showed better results with the Neo-Alphamill than with the conventional mill.
In bead milling, results vary with operating conditions and formulation. Please feel free to contact us below to discuss whether your material can be processed.